3x to 10x increase in Fatigue Life
40% Increase in Fatigue Strength
More effective weld repairs with greater MTBF and less issues with re-cracking
Two butt welds welded using identical parameters. The bottom plate had inter-run peening. Note the lack of distortion
The weld cap can be peened to impart residual compressive stresses to improve fatigue performance.
Produce a smoothly rounded corner with residual compressive stresses to massively increase the fatigue life and reduce cracking from edges of plate.
(click the image below for more details)
Companies that have purchase
Weight including tool: 1.25 kg
Length including tool: ~255 mm
Beats Per Minute: 6500
Vibration: 2.5 m/s2 (EN ISO 28927-10)
Noise level: 98 dB (A)
Air: 6 Bar, 330 l/min (Dry / lubricated air supply)
Bridges, Cranes, High Fatigue service equipment
Essential to achieve effective crack repairs
All the impact bits you need for any job